Suhu lan soldering wektu buzzer bakal langsung mengaruhi koefisien deformasi buzzer, saengga mengaruhi swara buzzer. Bisa uga nyebabake swara buzzer dadi cilik, ora ana swara, serak, lsp.
Kanggo ngindhari masalah ing ndhuwur, muga-muga bisa uga para pelanggan bisa ngrujuk tabel parameter proses sing adol kanggo njamin kualitas produksi.
Buzzer | Parameter Soldering | |||
Proses Soldering | Temp. (℃) | Wektu (sec.) | Kaping | |
Klebu | Refolw Soldering | 230 ± 10 | Ndhuwur 170 ℃ WET Wayahe 40 ~ 70 | 2 |
Timbal | Soldering gelombang | 245 ± 5 | 3 ~ 6 | 1 ~ 2 |
Soldering Manual | 330 ± 10 | 1 ~ 2 | 1 ~ 2 | |
Lead gratis | Refolw Soldering | 245 ± 15 | Ndhuwur 180 ℃ WET Wayahe 40 ~ 70 | 3 |
Soldering gelombang | 260 ± 5 | 4 ~ 8 | 2 ~ 3 | |
Soldering Manual | 350 ± 10 | 1 ~ 3 | 2 ~ 3 |